Bonding of dual-cured resin cement to zirconia ceramic using phosphate acid ester monomer and zirconate coupler


ファイル 記述 サイズフォーマット
JBMR77B_28_Ta&Fig.pdfTables&Figures34.61 kBAdobe PDF本文ファイル
JBMR77B_28_Text.pdfFullText59.74 kBAdobe PDF本文ファイル

タイトル: Bonding of dual-cured resin cement to zirconia ceramic using phosphate acid ester monomer and zirconate coupler
その他のタイトル: Zirconia ceramic primer using phosphate acid ester monomer and zirconate coupler
著者: Yoshida, Keiichi / Tsuo, Yukiko / Atsuta, Mitsuru
発行日: 2006年 4月
出版者: Wiley Periodicals, Inc.
引用: Journal of Biomedical Materials Research Part B: Applied Biomaterials 77B: 28-33, 2006
抄録: This study evaluated the shear bond strength between dual-cured resin luting cement and pure zirconium (99.9%) and industrially manufactured yttrium-oxide-partially-stabilized zirconia ceramic, and the effect of MDP (10-methacryloyloxydecyl dihydrogen phosphate) primer (MP) and zirconate coupler (ZC) on bond strength. Two different-shaped pure zirconium and zirconia ceramic specimens were untreated or treated with various primers, including different concentrations of MP containing phosphoric acid ester monomer (MDP) in ethanol, ZC containing a zirconate coupling agent in ethanol, or a mixture of MP and ZC. The specimens were then cemented together with dual-cured resin luting cement (Clapearl DC). Half of the specimens were stored in water at 37°C for 24 h and the other half were thermocycled 10,000 times before shear bond strength testing. The bond strengths of resin luting cement to both the zirconium and zirconia ceramic were enhanced by the application of most MPs, ZCs, and the mixtures of MP and ZC. For the group (MP2.0+ZC1.0) containing 2.0 wt % MP and 1.0 wt % ZC, no significant difference was observed between in shear bond strength before and after thermal cycling for both zirconium and zirconia ceramic (p > 0.05). For the other primers, statistically significant differences in shear bond strength before and after thermal cycling were observed (p < 0.05). The application of the mixture of MP and ZC (MP2.0+ZC1.0) was effective for bonding between zirconia ceramic and dual-cured resin luting cement. This primer may be clinically useful as an adhesive primer for zirconia ceramic restoration.
記述: This is a preprint of an article published in J Biomed Mater Res Part B: Appl Biomater 77B: 28-33, 2006
キーワード: bond strength / dual-cured resin cement / zirconia ceramic / MDP / zirconate coupler
URI: http://hdl.handle.net/10069/16668
ISSN: 15524973
DOI: 10.1002/jbm.b.30424
PubMed ID: 16193486
権利: Copyright (c) 2005 Wiley Periodicals, Inc.
資料タイプ: Journal Article
原稿種類: author
出現コレクション:130 学術雑誌論文

引用URI : http://hdl.handle.net/10069/16668

このリポジトリに保管されている文献はすべて著作権により保護されています。
印刷やダウンロード等データの複製は、調査研究・教育または学習を目的とする場合に限定されます。

 

Valid XHTML 1.0! Copyright © 2006-2015 長崎大学附属図書館 - お問い合わせ Powerd by DSpace